Publish Time: 2026-11-25 Origin: Site
Metal-oxide surge arresters are critical for protecting substation equipment from overvoltage transients. In coastal and heavily industrialized areas, the external insulation of these arresters must withstand contamination that promotes surface leakage current and flashover risk. While porcelain housings have been deployed for decades, silicone rubber composites have emerged as the preferred solution for severe pollution conditions due to their water-repellent surface and superior pollution performance .
The primary advantage of silicone rubber in polluted environments lies in its surface chemistry. The material exhibits inherent hydrophobicity, causing water to bead into discrete droplets rather than forming a continuous conductive film. This property significantly suppresses leakage current under wet conditions . More importantly, silicone rubber possesses the ability to transfer its hydrophobicity to accumulated contaminants—a phenomenon known as hydrophobicity transfer. Low-molecular-weight siloxane chains migrate through the pollution layer, rendering the contaminant surface water-repellent as well . This mechanism enables silicone arresters to maintain dielectric integrity even when coated with salt or industrial dust, potentially allowing for reduced creepage distances or extended cleaning intervals compared to porcelain alternatives .
In coastal regions, salt fog presents a persistent challenge. Independent testing has verified that 100% silicone rubber housings resist UV degradation and temperature extremes from -70°C to +200°C, while providing increased creep distance suitable for salt fog environments . Additionally, silicone arresters are significantly lighter than porcelain equivalents and fail in a non-shattering mode under overload, reducing collateral damage risk during installation and operation .
Despite these advantages, hydrophobicity is not a permanent characteristic. Three synergistic factors drive degradation in service:
Electrical discharge activity: In polluted conditions, leakage current generates dry-band arcing. Localized temperatures exceeding 300°C break Si-O and Si-C bonds in the polymer backbone, permanently reducing the material's recovery capacity. Surfaces transition from hydrophobic (HC1–HC2) toward hydrophilic (HC5–HC6) states .
Environmental contamination: While silicone can encapsulate moderate contamination, severe acidic pollutants (NOx, SOx) chemically attack the siloxane backbone through hydrolysis, destroying the recovery mechanism .
Ultraviolet radiation: Prolonged UV exposure causes photo-oxidation and chain scission at the surface, creating a brittle, chalky layer that impedes migration of low-molecular-weight chains from the bulk material .
A condition-based maintenance approach is recommended, integrating periodic assessment with targeted intervention.
Hydrophobicity should be evaluated using the spray method according to IEC TS 62073, classifying surfaces from HC1 (completely hydrophobic) to HC7 (completely hydrophilic). Measurements should be conducted during dry periods to avoid confounding effects of surface moisture. Particular attention should be directed to the underside of sheds and areas near the high-voltage terminal, where electric field concentration accelerates aging .
4.2 Cleaning Protocols
When contamination accumulation exceeds acceptable equivalent salt deposit density thresholds, cleaning is warranted. Dry cleaning methods (compressed air or soft brushing) are preferred for lightly contaminated surfaces. For more tenacious deposits, low-pressure washing with demineralized water is recommended, followed by a recovery period to allow hydrophobicity to re-establish before re-energization.
If hydrophobicity assessment reveals persistent HC5–HC7 classification after cleaning, restoration measures should be considered. Application of RTV silicone coatings can temporarily restore surface water repellency, though coating thickness and adhesion require careful control . For severely aged housings where recovery is not achievable, replacement planning should be initiated. Recent research has demonstrated that superhydrophobic coatings based on PDMS and nano-silica can achieve contact angles exceeding 159° and significantly reduce leakage current, offering a potential retrofit solution for aging arresters .
Silicone rubber arresters provide measurable performance advantages in high-pollution and coastal environments through their hydrophobicity and hydrophobicity transfer capabilities. However, these properties require active management. A maintenance program combining periodic hydrophobicity classification, appropriate cleaning, and timely restoration can extend service life and ensure reliable overvoltage protection. As contamination severity increases and aging progresses, the balance between maintenance investment and replacement cost should be reassessed using accumulated condition data.
Home Products Solutions Technical Resources News Sustainability About Us Contact
Surge Arrester Insulator Fuse Break Switch Overhead Line Hardware Fittings Cable Accessories